There’s a lot more to the extruder than making strap handles. With a multitude of commercial dies or custom homemade extruder dies, the only limit is the imagination. In this post, an excerpt from his video The Extruder Video: Getting the Most Out of Your Clay Extruder, Daryl Baird shows how he dresses up an ordinary extruded tray with trim made from a custom credit card die.- Jennifer Poellot Harnetty, editor
Assemble it correctly. Make sure your extruder is assembled correctly, according to the manufacturer's instructions.
If you bought a used or custom-made extruder, ask the person who sold it to you to cover the operation basics, if possible.
Use moist clay that has been wedged well. This can't be overstated. Just about any clay can be pushed through an extruder, but the results will vary enormously, depending on the characteristics of each. Clearly some clay bodies are
better suited to extruder work than others. As a general rule, any clay in a condition that is well suited for use on a potter's wheel will work well in your extruder. This is not to say that you can't use fresh clay right out of the bag. But
if it has been around awhile and it seems a little stiff, it will be more difficult to use in your extruder. You shouldn't have to exert superhuman force to get the clay to move through the die.
Practice, practice, and more practice. Just about every tool or instrument requires some practice if you're going to master it. If you're new to extruding, give yourself and the extruder a chance.
Working alone? Use the chest press method. Under fill the barrel so the handle is lower and closer to the barrel when you start. Now, standing directly in front of the extruder, square up your stance and press the handle with the
center of your chest. This frees both of your hands to guide the clay as it extrudes.
Cut off the first few inches. The first part of an extrusion never seems to come out straight. Cut it off squarely, then finish your extrusion. If you're making a hollow extrusion, you can help it to come out straighter by pressing
your flattened hand with slight upward pressure against the bottom of the extrusion as you pull on the handle with your other hand.
Search the Daily
Published Jan 24, 2025
This clip was excerpted from The Extruder Video: Making the Most Out of Your Clay Extruder, which is available in the Ceramic Arts Network Shop!
Five Extruder Tips from Daryl!
**First published in 2015.
Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Related Content
Ceramic Artists
Functional Pottery
Ceramic Sculpture
Glaze Chemistry
High-Fire Glaze Recipes
Mid-Range Glaze Recipes
Low-Fire Glaze Recipes
Ceramic Colorants
Ceramic Glazes and Underglazes
Ceramic Raw Materials
Pottery Clay
Ceramic Decorating Tools
Ceramic Kilns
Making Clay Tools
Wheel Throwing Tools
Electric Kiln Firing
Gas Kiln Firing
Raku Firing
Salt Firing and Soda Firing
Wood Kiln Firing
Ceramic Decorating Techniques
Ceramic Glazing Techniques
Handbuilding Techniques
Making Ceramic Molds
Making Ceramic Tile
Wheel Throwing Techniques