Molds are a simple way to create simple or complex forms that allow you to make multiple copies of a form with little effort. When you do this, the individual forms lose their preciousness, which allows you the freedom to creatively experiment. And as you build a library of forms, you’ll find even greater flexibility as you cut and reassemble shapes in any number of configurations. Guy Michael leads you step-by-step through the entire mold making and slip casting process. By the end of his demonstration, you’ll understand the principles of making both single and multi-part molds as well as how to make your own slip and successfully cast pieces.

Contents:
Introduction
Chapter 1 - Basic Tools
Chapter 2 - Simple Molds
Chapter 3 - Multiple Piece Molds
Chapter 4 - Mixing & Pouring Casting Slip
Chapter 5 - Joining Cast Pieces
Conclusion

Total runtime: Approximately 1 hour, 29 minutes

Gallery

About the Author

Guy Michael Davis

Guy Micheal Davis holds a BFA from the Kansas City Art Institute and an MFA from The Ohio State University. His work has been exhibited internationally and he has participated in residencies at the Richard Carter Studio, Pope Valley, California; Dresden Porcelain Manufactory, Dresden, Germany; and Walbzrych Porcelain Factory, Walbzrych, Poland. He is currently an adjunct faculty member at the University of Cincinnati and a member of Future Retrieval, a collaboration with artist Katie Parker. To learn more about Guy Michael Davis, please visit guymichaeldavis.blogspot.com. To learn more about Future Retrieval, please visit futureretrieval.blogspot.com.
Unfamiliar with any terms in this video? Browse our glossary of pottery terms!
Load more comments
Thank you for the comment! Your comment must be approved first
avatar
Log In or Sign Up to be able to comment