Naysan McIlhargey’s Recipes

Corien Ridderikhoff’s Recipe

4 Corien Ridderikhoff’s small vase, 21/2 in. (6.5 cm) in height, cast porcelain, crackle glaze, fired to 2246°F (1230°C) in oxidation, 2021.
4 Corien Ridderikhoff’s small vase, 21/2 in. (6.5 cm) in height, cast porcelain, crackle glaze, fired to 2246°F (1230°C) in oxidation, 2021.

1 Naysan McIlhargey’s Westside Brewery 275 Steins, 9 in. (23 cm) in height each, stoneware, Celadon #5 glaze, gas fired, 2022.
1 Naysan McIlhargey’s Westside Brewery 275 Steins, 9 in. (23 cm) in height each, stoneware, Celadon #5 glaze, gas fired, 2022.
2 Naysan McIlhargey’s pieces, Nigel Wood White Base Glaze, various painted stains and oxides, 2015–2022.
2 Naysan McIlhargey’s pieces, Nigel Wood White Base Glaze, various painted stains and oxides, 2015–2022.

3 Naysan McIlhargey’s pieces with Earlham College (E.C.) Black (a tenmoku glaze), all tenmoku pieces wood fired, 2017–2022.
3 Naysan McIlhargey’s pieces with Earlham College (E.C.) Black (a tenmoku glaze), all tenmoku pieces wood fired, 2017–2022.

Unfamiliar with any terms in this article? Browse our glossary of pottery terms!
Topics: Ceramic Artists
Click the cover image to return to the Table of Contents

You have read 1 of 3 of your complimentary articles for the month.

For unlimited access to Ceramics Monthly premium content, please subscribe.

Yes, I want to subscribe to Ceramics Monthly

Not right now. Continue to article.

We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.