All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 30.00
calcined-epk 20.00
thiele-kaolin 50.00

Instructions

Thiele kaolin needs to be applied very thinly, so the consistency of the slip should be a little thicker than skim milk. I recommend one quick dip only. If this is applied thick or has excess drips, the slip will craze and fall off the pot after firing. 

This recipe was shared by Eric Ordway in the December 2025 issue of Ceramics Monthly.