All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gillespie Borate 47.60
Talc 9.50
Grolleg 19.10
Silica 23.80
Add Amount
Rutile 15.00

Instructions

Intended to be used as an effect glaze, this works really well layering with others, but not as a solo glaze. High flux.

This recipe was shared by Riley Rist in the October 2025 issue of Ceramics Monthly.