All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 8.70
Whiting 7.61
Ferro Frit 3134 18.48
Custer Feldspar 38.04
silica 27.17
Add Amount
BENTONITE 5.43
Bone Ash 1.09
Copper Carbonate 1.63
tin-oxide 8.70
Zinc Oxide 4.35
Shark Fin Recipe

Instructions

This glaze has a tendency to gel, so add a little sodium silicate as needed. The recipes was generated by OpenAI’s machine learning software GPT-2 as part of Derek Au’s This Vessel Does Not Exist project: www.derekau.net/this-vessel-does- not-exist/2021/3/22/generated-glazes-real. 

 

This recipe was shared by Mariana Baquero in the Nov/Dec 2022 issue of Pottery Making Illustrated.