All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 3.70
Whiting 10.40
Ferro Frit 3124 9.50
Nepheline Syenite 39.70
EPK Kaolin 14.20
Silica 19.70
Zinc 2.80
Add Amount
Zircopax 10.00
Bentonite 2.00

Instructions

I adjusted the this recipe by replacing talc with some nepheline syenite and dolomite. I suspect this glaze may take colorants well based on a few tests I have done. It looks best when slow cooled. I adapted this recipe, with a couple of adjustments, from John Britt’s book The Complete Guide to Mid-Range Glazes. 

This recipe was shared by Kyla Strid in the January 2025 issue of Ceramics Monthly.