All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Barium 2.00
Whiting 19.60
Custer Feldspar 24.50
Grolleg 19.60
Silica 34.30
Add Amount
Tin Oxide 1.00
Yellow Iron 0.50

Instructions

One of the best, pure blue-green celadons I’ve ever used, both for color and opacity. It’s great on buff clays too. For soda kilns, it needs to be fired to a hot cone 10. Cone 11 is ideal.

This recipe was shared by Ben Eberle in the December 2025 issue of Ceramics Monthly.