All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
wood-ash-(unwashed) 41.50
Custer Feldspar 34.50
silica 24.00

Instructions

This glaze presents a wonderful white that breaks black over stoneware clays. Over clays with greater iron content, the glaze will go more blue. Best applied by dipping. Should be applied fairly thickly, but if applied too thick will present pink blushing. 

 

This recipe was shared by Erik Wilson in the July/August 2023 issue of Pottery Making Illustrated.