All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 14.05
strontium carbonate 1.11
Whiting 16.88
Ferro frit 3195 7.63
Custer Feldspar 15.31
EPK Kaolin 16.51
silica 28.51
Add Amount
BENTONITE 2.00

Instructions

This is an excellent glaze to use over surface texture. It pools beautifully and allows even fine details to show through. You may wish to experiment with other colorants and Mason stains. 

 

This recipe was shared by Carol Harris in the July/August 2023 issue of Pottery Making Illustrated.