All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 47.60
Grolleg 47.60
Titanium Dioxide 4.80

Instructions

Deep orange flashing with strong carbon trapping tendencies and blue titanium hints. This glaze is great with soda and even better with wood. Apply in a thin milky consistency. Medium to light soda interaction is preferred. Fire to cone 10 and up—does not run.

 

This recipe was shared by Samuel Newman in the December 2024 issue of Ceramics Monthly.