All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
soda ash 16.32
nepheline syenite 38.64
soda feldspar 9.31
epk kaolin 17.01
Cedar Heights Redart Clay 5.71
om4 ball clay 13.01

Instructions

Note: There are many variations of Malcolm Davis Shino glaze, with alterations made based on clay body being used. 

 

This recipe was shared by Dan Anderson in the March 2022 issue of Ceramics Monthly.