All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
water-(in-gal) 1.00
sodium-silica-(in-tbsp) 3.00
soda-ash-(in-tsp) 1.50

Instructions

Mix the soda ash into warm water to dissolve, then add the sodium silicate. Magic water can be used instead of slip when joining handles or other attachments. It requires less cleanup than slip and helps prevent cracks from forming along the joints. 

 

This recipe was shared by Mark Arnold in the September 2022 issue of Ceramics Monthly.