All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
dolomite 5.20
whiting 16.80
custer feldspar 32.00
epk kaolin 14.10
silica 31.90
Add Amount
mason stain #6464 3.60

Instructions

Mix to a heavy-cream consistency. Also works to make color variations, with other stains replacing the yellow Mason stain. Test to find appropriate percentage for the desired color. 

This recipe was shared by Abby Reczek in the February 2022 issue of Ceramics Monthly.