All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Instructions

This well-known ash glaze, associated with the Leach Pottery at St Ives, presents a lighter green color over iron-bearing stonewares. Pairs nicely with white slip. Apply by dipping or pouring. This glaze applies more smoothly than the basic ash glaze. 

 

This recipe was shared by Erik Wilson in the July/August 2023 issue of Pottery Making Illustrated.