All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
laurel-wood-ash 20.00
cerromina 80.00

Instructions

Cerromina is a low-melting-temperature clay I get from the central valley of Costa Rica. The recipe looks best with a sprayed application in a slow-cool firing to cone 6 in an electric kiln. 

 

This recipe was shared by Matias Braun in the June/July/August 2024 issue of Ceramics Monthly.