All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
liquid-sodium-silicate-(in-tbsp) 3.00
soda-ash-(in-tsp) 1.50
water-(in-gal) 1.00

Instructions

This recipe makes quite a large batch. I normally cut it in half. 

 

This recipe was shared by Carol Harris in the July/August 2023 issue of Pottery Making Illustrated.