All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 16.80
strontium carbonate 12.00
Wollastonite 6.40
nepheline syenite 24.00
EPK Kaolin 8.00
silica 32.80
Add Amount
BENTONITE 2.00

Instructions

This glaze is very clear even over a dark clay body, unless applied thickly.

This recipe was shared by Evelyn Ward in the April 2023 issue of Ceramics Monthly.