All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 16.80
Wollastonite 6.40
nepheline syenite 24.00
strontium carbonate 12.00
EPK Kaolin 8.00
silica 32.80
Add Amount
BENTONITE 2.00

Instructions

This recipe was shared by Margaret Kinkeade in the March/April 2023 issue of Pottery Making Illustrated.