All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Baking Soda 2.00
Borax 0.50
Soda Ash 2.00
Water 4.00

Instructions

Note: baking soda, borax, and soda ash are measured in pounds; water is measured in gallons.

I use this solution in cone 2–12 soda and wood firings and spray it in. 

 

This recipe was shared by Justin Rothshank in the June/July/August 2022 issue of Ceramics Monthly.