All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
ferro frit 3110 50.00
epk kaolin 50.00
Add Amount
mason stain #6300 50.00

Instructions

Mix to a heavy-cream consistency. This stain works best when applied under glazes. Apply before bisque firing. 

This recipe was shared by Abby Reczek in the February 2022 issue of Ceramics Monthly.