All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Copper Oxide 89.00
frit-(alkaline-or-borax-frit) 9.00
BENTONITE 2.00

Instructions

This glaze has a low melting point, and will mature in about an hour. 

 

This recipe was shared in the January/February 2023 issue of Pottery Making Illustrated.