All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
kona f-4 feldspar 25.97
Grolleg Kaolin 48.17
pyrotrol 8.62
silica 17.24
Add Amount
BENTONITE 10.50

Instructions

I use Mason stains to color this slip, which I mix by eye and then test. One of my favorites is Ivy (MS6223), which I use in varying degrees for different shades of green. I also love Turquoise (MS6364). I combine this with black stain for a slate blue slip.

*Substitute Minspar 200 feldspar for the Kona F-4 feldspar. 

This recipe was shared by Evelyn Ward in the April 2023 issue of Ceramics Monthly.