All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Whiting 19.80
Ferro Frit 3124 19.80
Nepheline Syenite 19.80
EPK Kaolin 19.80
Silica 20.80

Instructions

Dip or spray a thin application of this glaze over the entire piece.

 

This recipe was shared by Stephanie Wilhelm in the May/June 2024 issue of Pottery Making Illustrated.