All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3124 70.00
EPK Kaolin 30.00

Instructions

These recipes were shared in Low Fire Soda by Justin Rothshank, published by The American Ceramic Society, and in the October 2024 issue of Ceramics Monthly.