All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Ferro Frit 3134 30.00
Ferro Frit 3195 45.00
EPK Kaolin 25.00

Instructions

This was a Nova Scotia College of Art and Design (NSCAD) shop glaze when I was a student. It’s transparent and glossy, and I dip or brush this glaze thinly to avoid cloudiness. When desired, I apply over areas decorated with underglaze or colorant illustrations to add extra gloss. 

This recipe was shared by Lindsay Montgomery in the November 2025 issue of Ceramics Monthly.