All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Barium Oxide 10.00
Whiting 10.00
Nepheline Syenite 80.00
Add Amount
Cobalt Oxide 0.50
Red Iron Oxide 3.00

Instructions

Published in "A Lifelong Relationship" by Jan de Rooden, in the May 2000 issue of Ceramics Monthly.