All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Calcium Borate 10.00
Calcium Carbonate 9.00
Dolomite 3.00
Zinc 1.00
Barium Carbonate 2.00
Feldspar 65.00
Silica 10.00
Add Amount
Copper Carbonate 5.00
Titanium 5.00

Instructions

Excerpted from The Ceramic Spectrum by Robin Hopper. Published by The American Ceramic Society and available for purchase in the Ceramic Arts Network Shop, mycan.ceramicartsnetwork.org/s/shop.

 

This recipe was shared by Robin Hopper in the January 2024 issue of Ceramics Monthly.