All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Magnesium Carbonate 50.00
nepheline syenite 50.00
Add Amount
BENTONITE 2.00

Instructions

This recipe was shared by AL Holen in the Nov/Dec 2022 issue of Pottery Making Illustrated.