All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 1.00
Lithium Carbonate 1.00
Water 2.00

Instructions

Note: Gerstley Borate and Lithium Carbonate are listed in cups. Water is listed in gallons.

Applied in 1–3 thin layers with a brush to the outer surface of the clay. Tends to settle, so be sure to mix well before application. 

 

This recipe was shared by Margaret Kinkeade in the March/April 2023 issue of Pottery Making Illustrated.