All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 23.60
nepheline syenite 71.60
Ball Clay 4.80
Add Amount
BENTONITE 4.00
cobalt carbonate 1.10
zircopax 4.80

Instructions

This is a very stable glaze. There are no special mixing requirements. 

This recipe was shared by Matthew Eames in the October 2022 issue of Ceramics Monthly.