All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
wood-ash-(unwashed) 60.00
Cornwall Stone 40.00

Instructions

Mix this wash very thin, only slightly thicker than water, and apply to bisqueware by dipping. It works well over a variety of slips. 

This recipe was shared by Ian Hall-Hough in the September 2023 issue of Ceramics Monthly.