All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 31.58
Grolleg Porcelain 52.63
locally-harvested-clay 5.26
Tile 6 10.53

Instructions

Applied to a majority of my work, this slip yields bright oranges, yellows, and browns (dependent on harvested clay). The harvested clay I use is a high-iron, low-fire clay body. I generally ball mill this slip and apply it to bisqueware.

 

This recipe was shared by Johnny Arvizu in the February 2024 issue of Ceramics Monthly.