All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Feldspar 8.90
kona f-4 feldspar 6.30
EPK Kaolin 8.90
fhc-(spinks) 8.90
cedar-heights-gold-art 8.90
lincoln-fire-clay 8.90
lizella 17.90
newmans-red 8.90
OM-4 Ball Clay 8.90
silica 13.50

Instructions

It is an odd recipe, with a lot of ball clay (FHC and OM-4), but the Lizella and Lincoln clays have so much tooth that I still only have 11% shrinkage from the plastic-clay stage through firing to

cone 10. 

 

This recipe was shared by AL Holen in the Nov/Dec 2022 issue of Pottery Making Illustrated.