Yoko Sekino-Bove's N502 Yoko Sekino-Bove

You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesAlready a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Please enjoy this complimentary recipe for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesNot right now. Continue to recipe. Already a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Subscribe
Ingredients
Instructions
Published in "Expanding Your Palette in Mid-Range Firing" by Yoko Sekino-Bové, in the Jan 2011 issue of Ceramics Monthly.
The test batch for this glaze was 300g, with a tablespoon of epsom salts added as a flocculant.
Fire in an electric kiln, in an oxidation/neutral atmosphere.
Recipe Topics
Clay Bodies and Casting Slips
Low Fire (Cone 022 – 01)
Mid Range (Cone 1 – 7)
High Fire (Cone 8 – 14)
Raku
Salt, Soda, and Wood
Slip, Engobe, and Terra Sigillata
Reference
Create your own Recipes!
You can keep your recipes private or share with others.
Create a Recipe
Manage your Recipes