All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Nepheline Syenite 31.60
Ball Clay 63.20
Silica 5.20
Add Amount
Tin Oxide 5.30
Titanium Dioxide 10.50

Instructions

Published in "Blending the Lines" by Kenyon Hansen, in the Jul/Aug 2014 issue of Pottery Making Illustrated.