All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Wood Ash 46.51
Custer Feldspar 46.51
Silica 6.98

Instructions

This recipe was shared by Hanako Nakazato in the June/July/August 2018 issue of Ceramics Monthly.