All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 14.29
Washed Wood Ash 28.57
Custer Feldspar 33.33
OM 4 Ball Clay 23.81
Add Amount
Bentonite 2.00

Instructions


I apply this glaze over slip decoration. A thin application promotes a more defined slip deco- ration while a thicker application mutes the slip under a fat, buttery transparency.

This recipe was shared by Jason Hartsoe in the September/October 2021 issue of Pottery Making Illustrated.