All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 35.00
Ferro Frit 3110 65.00

Instructions

Published in "From Oh No! to Oh Wow!" by Kate and Will Jacobson, in the Sep/Oct 2011 issue of Pottery Making Illustrated.
Apply thin or thick over dry sacrificial or breakaway slip.