All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Custer Feldspar 25.00
EPK Kaolin 25.00
OM 4 Ball Clay 25.00
Silica 25.00
Add Amount
Zircopax 5.00

Instructions


If applied to bone-dry ware by brushing, a fine crackle pattern can appear in the surface of the slip.