White Salt Moloney Hi

You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesAlready a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Please enjoy this complimentary recipe for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesNot right now. Continue to recipe. Already a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Subscribe
Ingredients
Instructions
Published in "Glazes for Latex Resist" by Courtney Martin, in the Dec 2013 issue of Ceramics Monthly.
I fired these glazes to cone 10 in my wood kiln, and add 4-8 pounds of salt. When I've fired these glazes in friends' kilns, I've found that they also like hotter and saltier atmospheres. These are all very stable and I don't have any trouble with them running.
I add Epsom salts to each of these glazes. I like the way it helps keep the glaze in suspension, and I feel like it makes the glaze stronger after it is on the pot and before it's fired. Without the Epsom salts, I find the glaze to be dusty and hard to paint wax over.
Recipe Topics
Clay Bodies and Casting Slips
Low Fire (Cone 022 – 01)
Mid Range (Cone 1 – 7)
High Fire (Cone 8 – 14)
Raku
Salt, Soda, and Wood
Slip, Engobe, and Terra Sigillata
Reference
Create your own Recipes!
You can keep your recipes private or share with others.
Create a Recipe
Manage your Recipes