All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Fukushima Feldspar (substitute: Custer Feldspar 57.00
Gray Limestone (substitute: Whiting) 31.50
Ball Clay 11.50
Add Amount
Zirconium Silicate 10.30

Instructions

Published in "Fumiya Mukoyama's Zogan Yusai" by Naomi Tsukamoto, in the Jan/Feb 2010 issue of Pottery Making Illustrated.
Fired to 2264°F (1240°C) in a gas kiln—in an oxidizing atmosphere.