All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Barium Carbonate 14.90
Gerstley Borate 40.50
Nepheline Syenite 33.80
Silica 10.80

Instructions

Published in "Fish Tales" by Lisa Merida-Paytes, in the Jul/Aug 2009 issue of Pottery Making Illustrated.