All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gerstley Borate 50.00
Mason Stain 50.00

Instructions

Published in "Low-Fire Glazes" by Lauren Karle, in the October 2016 issue of Ceramics Monthly.
Mix by volume. This wash give you more intense colors than adding Mason stains to slip. You do not need to add deflocculant to the wash.