All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Barnard Slip 75.00
Minspar 200 Feldspar 25.00

Instructions


I like using this glaze for its softness. It is a nice matte black with a lot of variety in the surface it produces. I’ve dipped pots in this glaze, but get the best results when it’s sprayed until a heavy dusting is applied to the pot. Be careful not to apply too thick because it will crack off. In light reduction, the surface will be more uniform, but a heavier reduction will provide more texture and movement.

This recipe was shared by Antonio Martinez in the September 2020 issue of Ceramics Monthly.