All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Gillespie Borate 18.95
Whiting 2.11
Ferro Frit 3134 26.32
Nepheline Syenite 26.32
EPK Kaolin 10.51
Silica 15.79
Add Amount
Tin Oxide 5.26
Zinc Oxide 5.26

Instructions

This glaze comes from Val Cushing (when you see V.C. in any recipe title, it probably refers to Cushing). The glaze breaks nicely over textured areas. I use it as a liner glaze on my vessel forms.

Originally published in the October 2017 issue of Ceramics Monthly.