All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Hawthorne Bond 40.00
KT #1-4 20.00
New Foundry Hill Creme 20.00
Custer Feldspar 12.00
Silica 8.00

Instructions

The clay is the shop mix used at the University of Nebraska-Lincoln.