Turquoise Matte Susan Beiner

You have read of of your complimentary recipes for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesAlready a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Please enjoy this complimentary recipe for the month.
For unlimited access to Ceramics Recipes premium content, please subscribe.
Yes, I want to subscribe to Ceramics RecipesNot right now. Continue to recipe. Already a digital subscriber? Log in now.
We understand your email address is private. You will receive emails and newsletters from Ceramic Arts Network. We will never share your information except as outlined in our privacy policy. You can unsubscribe at any time.

Subscribe
Ingredients
Instructions
This recipe was shared by Susan Beiner in the December 2018 issue of Ceramics Monthly.
This glaze is applied in a medium-thick application and fired to a hot cone 6 in a gas kiln. This glaze is not food safe.
I use several heavily fluxed base glazes combined with a variety o Mason stains, rare earth oxides, and encapsulated pigments to create palettes of color to glaze in a more painterly manner. Multiple glazes overlap, which influences how the glazes move across the forms. I am continually testing glazes and looking for interesting overlaps. Glaze application is done with a spray gun and bulb syringe. I draw glaze using a bulb syringe to further increase the mixing and melting of the glazes.
Recipe Topics
Clay Bodies and Casting Slips
Low Fire (Cone 022 – 01)
Mid Range (Cone 1 – 7)
High Fire (Cone 8 – 14)
Raku
Salt, Soda, and Wood
Slip, Engobe, and Terra Sigillata
Reference
Create your own Recipes!
You can keep your recipes private or share with others.
Create a Recipe
Manage your Recipes