All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Dolomite 10.00
Whiting 9.00
Soda Feldspar 25.00
Custer Feldspar 20.00
EPK Kaolin 18.00
Talc 6.00
Silica 12.00
Add Amount
Bentonite 2.00
Cobalt Carbonate 4.00
Lithium Carbonate 2.00

Instructions

Published in "E Unum Pluribus" by Kristina Bogdanov, in the Sep/Oct 2009 issue of Pottery Making Illustrated.