All recipes are displayed as ratios, unless "in parts" is included in the recipe. You can adjust the recipe for larger or smaller batches by adjusting the total below the recipe. For example, for a 10,000-gram batch, put “10,000” in the box. Have more questions? View our help page here or watch a video tutorial here. 

Ingredients

Ingredient Amount
Barium Carbonate 4.04
Gerstley Borate 4.62
Magnesium Carbonate 4.04
Whiting (Pfizer Vicron 41-8) 14.43
Ferro Frit 3195 1.01
Custer Feldspar 41.56
EPK Kaolin 4.33
Silica 25.97
Add Amount
Tin Oxide 0.87
Zinc Oxide 1.73
Copper Carbonate 0.43
Bentonite 1.01

Instructions

Published in "Cone 9 Glazes," in the March 2016 issue of Ceramics Monthly.

The piece in the image shown here has multiple glazes on it, including Tom Turner's Flambe, Blue Teadust, and a wash of iron oxide and water.
Flambe glazes cannot be applied thin.